English: Tensile properties of the Fe–55Mn–3Al–3Si wt% TWIP steel as a function of the test temperature; strain rate ε=10-4.s-1.
فارسی: خواص کششی فولاد تویپ Fe–55Mn–3Al–3Si wt% به عنوان تابعی از دما؛ نرخ کرنش ε=10-4.s-1
Date
Source
Own work Data from: Georg Frommeyer, Udo Brüx and Peter Neumann, Supra-Ductile and High-Strength Manganese-TRIP/TWIP Steels for High Energy Absorption Purposes, ISIJ International, Vol. 43 (2003) pp. 438-446.
to share – to copy, distribute and transmit the work
to remix – to adapt the work
Under the following conditions:
attribution – You must give appropriate credit, provide a link to the license, and indicate if changes were made. You may do so in any reasonable manner, but not in any way that suggests the licensor endorses you or your use.
share alike – If you remix, transform, or build upon the material, you must distribute your contributions under the same or compatible license as the original.
{{Information |Description ={{en|1=Tensile properties of the Fe–55Mn–3Al–3Si wt% TWIP steel as a function of the test temperature; strain rate ε=10<sup>-4</sup>.s<sup>-1</sup>.}} {{fa|1=خواص کششی [[:fa:فولاد ت...